International Journal of Advances in Mechanical and Civil Engineering (IJAMCE)
.
Follow Us On :
current issues
Volume-11,Issue-1  ( Feb, 2024 )
Past issues
  1. Volume-11,Issue-1  ( Feb, 2024 )
  2. Volume-10,Issue-6  ( Dec, 2023 )
  3. Volume-10,Issue-5  ( Oct, 2023 )
  4. Volume-10,Issue-4  ( Aug, 2023 )
  5. Volume-10,Issue-3  ( Jun, 2023 )
  6. Volume-10,Issue-2  ( Apr, 2023 )
  7. Volume-10,Issue-1  ( Feb, 2023 )
  8. Volume-9,Issue-6  ( Dec, 2022 )
  9. Volume-9,Issue-5  ( Oct, 2022 )
  10. Volume-9,Issue-4  ( Aug, 2022 )

Statistics report
Apr. 2024
Submitted Papers : 80
Accepted Papers : 10
Rejected Papers : 70
Acc. Perc : 12%
Issue Published : 58
Paper Published : 1075
No. of Authors : 2871
  Journal Paper


Paper Title :
Innovative Bonding Agent of Steel Bars in Concrete Made from High Calcium Fly Ash Geopolymer Mortar Containing Hybrid Cement

Author :Darakorn Intarabut, Hattakorn Sodrum, Tanapoom Ongloy, Tanakorn Phoo-Ngernkham

Article Citation :Darakorn Intarabut ,Hattakorn Sodrum ,Tanapoom Ongloy ,Tanakorn Phoo-Ngernkham , (2018 ) " Innovative Bonding Agent of Steel Bars in Concrete Made from High Calcium Fly Ash Geopolymer Mortar Containing Hybrid Cement " , International Journal of Advances in Mechanical and Civil Engineering (IJAMCE) , pp. 71-74, Volume-5,Issue-2

Abstract : This article presented the influence of hybrid cement (HPC) replacement, sand-to-binder ratio, sodium silicate-to-sodium hydroxide solutions (Na2SiO3-to-NaOH ratio) and liquid alkaline-to-binder ratio on compressive strength of high calcium fly ash (FA) geopolymer mortar. The FA was replaced with HPC at the ratios of 100:0, 90:10, 80:20and 70:30.The sand-to-binder ratioof 0.5, 1.0, 1.5,Na2SiO3-to-NaOH ratios of 1.0, 2.0, 2.5,and liquid alkaline-to-binder ratios of 0.45, 0.55, 0.60, 0.65,were also tested.Constants14M NaOH concentration was used in all mixes.Test results indicated that the compressive strength tended to increase with increase of HPC replacement. The compressive strength of geopolymer mortars at sand-to-binder ratiosof 0.5, 1.0, liquid alkaline-to-binder ratios of 0.45, 0.55 and Na2SiO3-to-NaOH ratio of 2.5, were the best results. Therefore, all of FA geopolymer mortar containing HPC with different sand-to-binder ratio, liquid alkaline-to-binder ratio, Na2SiO3-to-NaOH ratio meet the requirement of chemical anchorage except Na2SiO3-to-NaOH ratio of 1.0. Keywords - Geopolymer, high calcium fly ash, hybrid cement,bonding agent,steel bars in concrete.

Type : Research paper

Published : Volume-5,Issue-2


DOIONLINE NO - IJAMCE-IRAJ-DOIONLINE-12303   View Here

Copyright: © Institute of Research and Journals

| PDF |
Viewed - 47
| Published on 2018-07-28
   
   